Intro to TIG Welding EP16 - Outside Corner Joint Aluminum

Jody Collier - Intro to TIG Welding • 4m 22s

Up Next in Jody Collier - Intro to TIG Welding

  • Intro to TIG Welding EP17 - 2F Lap Jo...

    In this video, we are TIG welding 11 ga cold rolled steel and using different diameters of filler rod.
    The first joint was welded using 3/32" filler rod at approximately 120 amps.
    A second lap joint was also shown using 1/16" at slightly lower amperage.