There are many different ways to tig weld a tee joint. In this video I show 3 different ways...straight dcen with no pulse using a foot pedal, 1 pulse per second with foot pedal floored at 131 amps, and pumping the foot pedal for sort of a manual pulse.
For 11ga cold rolled steel lap joints its all about torch angle and arc length.
Torch angle is pretty forgiving provided your arc length is tight.
So what is tight enough? The electrode diameter or less works for me
Fabricating a stainless steel part and talking about maintaining the corrosion resistance of stainless steel. Outside Corner joints using Aluminum angle backing
There is a technique for tig welding called "walking the cup".
While its mostly useful for pipe welding, it can also be a good technique for long runs on fillet welds.
In this video, I talk about cup size, electrode stickout, and how to hold the torch.
I set the lincoln TIG 200 to 177 amps and p...