TIG welding cold rolled steel 3"x3" x1/4" using er309L and E70s-6 filler metal.
12 outside joints provides plenty of welds to experiment using different size filler metals and pulse settings too.
There is also a second video of filling in the corners using silicon bronze.
Controlling the puddle, getting adequate penetration, avoiding undercut, preventing arc blow, and complying with AWS D1.1 acceptance criteria are all important.
Some welders are being required to test using 5/32" 7018 electrodes instead of smaller diameter electrodes like 1/8". 130 amps is at the...
Lots of Discussion happens when you talk about mig welding downhill. Personally, I prefer to go uphill on anything 3/16" and thicker. But for open butt root passes in pipe welding in fab shops, downhill mig is pretty common and yields good results provided the bevel, gap, fitup, and land are with...
JD and Jody experiment with a used welding positioner bought off ebay.
JD had just finished up a handrail project and had a few fittings and some pipe left over. They tried some 6" schedule 80 as well as some 1-1/2" sched 40 pipe on the positioner.
Always learning...