In this video, I go over mig welding settings for short circuit mig welding in horizontal and vertical uphill. Also a quick tip for vertical uphill settings. Arc shots and techniques are shown in detail.
For Out of position welding like vertical uphill, Short circuit mig welding requires some manipulation of the gun to prevent excess convexity of the bead profile. Dual shield flux core is different. This video shows the distinct difference in speed and bead profile
Science might say no but after a period of non use, rolling the tank sure seems to help the arc smooth out.
When you Mig weld after a long period of non use. It seems to help to roll the tank
In today's episode we'll be going over a D1.1 1G 1" thick welding plate. We'll be using .045 ER70S6. 1G Pulse Spray mig